GB-T1591 Q355E Steel Plate supplier
- Q355E Adopt standard: GB-T1591 Standard Specification is for Rolled Steels for Welded Structure
- Q355E Specification: Thickness: 1mm to 500mm; Width: 1500mm to 4500mm: Length: 3000mm to 27000mm
- Third Party Inspection for Q355E: ABS, DNV, BV, GL, CCS, LR, RINA, KR, NK, CE, SGS, IKE, IEI or other quality department.
- Q355E Chemical composition Max % of the Product analysis of grade
C | Si | Mn | P | S | Nb | V | Ti |
0.18 | 0.50 | 1.70 | 0.025 | 0.020 | 0.07 | 0.15 | 0.20 |
Cr | Ni | Cu | N | Mo | B | Als min | |
0.30 | 0.50 | 0.30 | 0.012 | 0.10 | – | 0.015 |
- Q355E Yield strength
Nominal thickness (mm) | To 16 | 16-40 | 40-63 | 63-80 | 80-
100 |
100-
150 |
150-
200 |
200-
250 |
250-
400 |
ReH – Minimum yield strength (MPa) | 345 | 335 | 325 | 315 | 305 | 285 | 275 | 265 | 265 |
- Q355E Tensile Strength
Nominal thickness (mm) | To 40 | 40-63 | 63-80 | 80-100 | 100-150 | 150-250 | 250-400 |
ReH – Minimum yield strength (MPa) | 470-630 | 470-630 | 470-630 | 470-630 | 450-600 | 450-600 | 450-600 |
- Q355E Impact Test degree and energy
Min Energy Nominal thickness | |||
Temperature ℃ | -40 | ||
Thickness (mm) | 12-150 | 150-250 | 250-400 |
Notch impact test. Min. absorbed energy | 34 | 27 | 27 |
- Equivalent grades of grade Q355E
- Q355E Delivery Time Or Lead Time: 15-30days
- Q355E Extra Service: Pretreatment (Shot Blasting, Sand Blast, Painting and Galvanized), Cutting Parts, Sample Service, Third Party inspection, UT Test and Size inspection.
- If you have any requirement in steel plate for Q355E, whether the new plate or stock list of material, please feel free to contact us by email of calling.
- If you had any question at our plate or service. Please contact our after service department to get faster reply.